1. Modeling the microstructural evolution during hot working of C-Mn and of Nb microalloyed steels using a physically based model
Sammanfattning : Recrystallization kinetics, during and after hot deformation, has been investigated for decades. From these investigations several equations have been derived for describing it. The equations are often empirical or semi-empirical, i.e. LÄS MER