Sökning: "Nickel based superalloys"
Visar resultat 16 - 20 av 48 avhandlingar innehållade orden Nickel based superalloys.
16. Low Cycle Fatigue and Thermo-Mechanical Fatigue of Uncoated and Coated Nickel-Base Superalloys
Sammanfattning : High strength nickel-base superalloys have been used in turbine blades for many years because of their superior performance at high temperatures. In such environments superalloys have limited oxidation and corrosion resistance and to solve this problem, protective coatings are deposited on the surface. LÄS MER
17. Oxidation induced failure of superalloys: High temperature crack growth and oxide scale properties
Sammanfattning : Gas turbine materials are designed to work in extreme environments in high temperature with an oxidising environment and variable mechanical loading. The study of high temperature fatigue properties of these materials is therefore important. LÄS MER
18. Influence of Microstructure in Machining of Nickel and Nickel-Iron Based Alloys
Sammanfattning : Superalloys are used in applications such as turbines, steam power plants and nuclear power systems in components that require good high temperature properties and/or corrosion resistance. They are classified as difficult-to-cut materials and hence, from a sustainable production point of view, tool wear and tool life are major factors when machining these alloys. LÄS MER
19. Weldability of Cast Superalloys - Effect of homogenization heat treatments on hot cracking susceptibility of cast Alloy 718, ATI® 718Plus®, and Haynes® 282®
Sammanfattning : Precipitation hardened Ni- and Ni–Fe-based superalloys are used in high-temperature sections of aero engines owing to their superior mechanical properties compared to those of the other alloys. However, their better mechanical performance is accompanied by its own challenges during the manufacturing process. LÄS MER
20. Creep modeling and first-principles investigation of high-temperature alloys
Sammanfattning : Stainless steels and nickel-based superalloys are materials that have been widely used to manufacture components servicing at high temperatures. Creep strength is one of the most important properties in such conditions. LÄS MER