Sökning: "Nickel based superalloys"
Visar resultat 6 - 10 av 48 avhandlingar innehållade orden Nickel based superalloys.
6. Weld Cracking in Precipitation Hardening Ni-based Superalloys
Sammanfattning : Manufacturing of hot structural components for aero engines requires the materials being used to be weldable. The high demands on strength and temperature resistance make nickel based superalloys the material of choice for this application. LÄS MER
7. Aluminide Diffusion Coatings for Ni Based Superalloys. Coating and Oxide Microstructure
Sammanfattning : This thesis reports on investigations of high temperature oxidation resistant aluminide diffusion coatings for Ni based superalloys. Such coatings basically consist of a .BETA.-NiAl layer at the surface of the . LÄS MER
8. Alloy Design and Characterization of γ′ Strengthened Nickel-based Superalloys for Additive Manufacturing
Sammanfattning : Nickel-based superalloys, an alloy system bases on nickel as the matrix element with the addition of up to 10 more alloying elements including chromium, aluminum, cobalt, tungsten, molybdenum, titanium, and so on. Through the development and improvement of nickel-based superalloys in the past century, they are well proved to show excellent performance at the elevated service temperature. LÄS MER
9. Microstructure of Pt modified aluminide diffusion coatings on Ni based single crystal superalloys
Sammanfattning : .... LÄS MER
10. Surface Integrity and Fatigue Performance of Nickel-based Superalloys
Sammanfattning : Due to global warming, the demand for more efficient gas turbines has increased. A way to achieve this, is by increasing the operating temperature of the gas turbine. Therefore, nickel-based superalloys have been developed to withstand these extreme temperatures and loads, especially in the hot sections. LÄS MER