1. An Insight into the Critical Role of Microstructure and Surface Preparation on Localized Conversion Coating Deposition on Cast Al Alloys
Sammanfattning : The spontaneous cerium conversion coating formation over aluminium alloys is affected by the chemical process conditions, the surface preparation prior to conversion treatment and the microstructure of the underlying alloy. Most research performed until now focus only on the former whereas the influence of the latter two is poorly understood. LÄS MER
2. Characterization of factors interacting in CGI machining : machinability - material microstructure - material physical properties
Sammanfattning : The Swedish truck industry is forced to find new material solutions to achieve lighter engines with increased strength. Customers and new environmental regulations demand both higher specific power and more environmentally friendly trucks, and this places a rising pressure on the manufactures. LÄS MER
3. Micro-structural based acoustic modelling of anisotropic open cell materials
Sammanfattning : A method for the calculation of the acoustic performance of open-cell foammaterials is discussed. From a known micro-structural geometry and theconstituent material, the relevant acoustic properties are computed using apreviously published analytical method for the calculation of the dynamicdrag impedance and a previously published method for the calculation of theelastic moduli. LÄS MER
4. Industrial Alloys Studied by Surface Sensitive Techniques
Sammanfattning : This thesis reports on surface studies of industrial materials whose importance for society manifests in the vast range of applications. In industrial materials alloying is performed in order to improve the parent material's physical and mechanical properties such as strength, corrosion and wear resistance, as well as high temperature performance in comparison to the pure metal. LÄS MER
5. Investigating the effect of extending powder particle size distribution of Ti-6Al-4V produced by powder bed fusion laser beam process : Influence of process parameters on material integrity
Sammanfattning : This thesis focuses on the topic of PBF-LB applied to titanium alloys. Of allalloys, an α + β is chosen, named Ti-6Al-4V. The selection of this particular alloy is driven by its current widespread use in many industrial applications where high strength coupled with low density are both desirable properties. LÄS MER