  1. 1. Cracks in superalloys

    Författare :Jonas Saarimäki; Johan Moverare; Kjell Simonsson; Magnus Hörnqvist Colliander; Robert Eriksson; Håkan Brodin; Mark Whitaker; Linköpings universitet; []
    Nyckelord :TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY;

    Sammanfattning : Gas turbines are widely used in industry for power generation and as a power source at hard to reach locations where other possibilities for electrical power supplies are insufficient. New ways of producing greener energy is needed to reduce emission levels. This can be achieved by increasing the combustion temperature of gas turbines. LÄS MER

  2. 2. Weldability and Testing Methodology in Precipitation Hardening Superalloys

    Författare :Jonny Jacobsson; []
    Nyckelord :TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; Weldability; Alloy 718; ATI® 718Plus™ and Haynes® 282®; Superalloys; Varestraint; Waspaloy®;

    Sammanfattning : Usable weldability data is desired in the manufacturing industry, especially within the aerospace industry where fabrication of structural jet engine components are realized. Welding of precipitation hardening superalloys such as Waspaloy®, Alloy 718, ATI® 718Plus™ and Haynes® 282® in particular can lead to solidification cracking in the fusion zone, liquation cracking in the heat affected zone and/or to solid state cracking. LÄS MER

  3. 3. Hot Cracking and Grain Boundary Weaknesses of Nickel - Based Superalloys

    Författare :Joel Håkan Andersson; Chalmers tekniska högskola; []
    Nyckelord :TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; Hot cracks; Notch rupture testing; Eutectic; Weldability; Varestraint testing; Grain boundary weaknesses; Superalloys;

    Sammanfattning : Abstract Grain boundary weaknesses of nickel-based superalloys not only materialize during service in the hot turbine engine sections but also during the weld manufacturing. The performance, in this respect, of the most commonly used alloys at Volvo Aero Corporation (VAC), 718 and the higher temperature capacity Waspaloy, are therefore the main subjects for this thesis. LÄS MER

  4. 4. Laser powder bed fusion processing and heat treatment of Ni-base superalloys: microstructure and properties

    Författare :Abdul Shaafi Shaikh; Chalmers tekniska högskola; []
    Nyckelord :TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; microstructure.; Additive manufacturing; heat treatment; Inconel 939; Haynes 282; superalloys; powder bed fusion – laser beam;

    Sammanfattning : Nickel-base superalloys are indispensable materials for the energy and aerospace industries. The additive manufacturing (AM) of these materials by powder bed fusion – laser beam (PBF-LB) presents a valuable opportunity to improve component performance and ease manufacturing and supply chain complexity in these industries. LÄS MER

  5. 5. Varestraint Weldability Testing of Cast Superalloys

    Författare :Sukhdeep Singh; Chalmers tekniska högskola; []
    Nyckelord :TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; Varestraint; Hot Cracking; Welding; Alloy 718; Cast Superalloys; ATI® 718 PlusTM; HIP;

    Sammanfattning : Precipitation hardened Ni- and Ni-Fe- based superalloys, used in hot structural components for aero engines, are subjected to hot cracking phenomena during manufacturing and specifically in welding. This type of cracking involves metallurgical reactions from the liquid phase in concomitance to weld restraints. LÄS MER